MATTER Undergraduate web site

 
  MATTERSteelMATTER | Site Map | Help | Contact us | Glossary | About  
 
     

Continue ]

Select process

  Raw materials     1 of 6
 

Raw materials

Raw materials do control much of the final chemistry of the steel, especially if we are using large amounts of recycled steel in the electric arc furnace.

 

 

 
  Raw materials | Steelmaking | Casting | Forming | Manufacturing | Products | Metallurgy
 
 

2000 MATTER, The University of Liverpool. All rights reserved.
    contact us   Last updated: July 25, 2000 commercial information