A student has made measurements of S1 from three films, from Debye Scherrer experiments on three different samples. It is known that all three samples are cubic. From the results determine the cubic structure type of each sample:

Use the data sheet here to help you.

Sample1

S1/mm

Sample2

S1/mm

Sample3

S1/mm

22 35 41
31 41 59
38 59 73
45 71 87
50 75 101
56 88 114
65 99 130
70 103 153
74 116 -
78 128 -